摘要
The interfacial Dzyaloshinskii-Moriya interaction (i-DMI) has been exploited in as-made symmetrical Au/[Fe/Au]n structures. By tailoring the chirality of the i-DMI at the Au/Fe interface, an overall enhancement of the i-DMI can be obtained in such a symmetrical structure. Furthermore, the tunability of the i-DMI was realized by changing the stacking number n. Compared to the top of Fe, a large tensile stress at the bottom of Fe due to lattice mismatch was responsible for the chirality change in the sub/Au/Fe system. Layer-resolved DMI calculations revealed that the sign of the spin-orbit coupling (SOC) energy was changed for Au near the interface of Au/Fe under tensile stress, subsequently reversing the chirality of the i-DMI from left-handed to right-handed. Our findings provide a simplest way to tune the i-DMI in a multilayer system, further benefiting the application of skyrmion-based devices.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 2665-2672 |
| 页数 | 8 |
| 期刊 | Nanoscale |
| 卷 | 13 |
| 期 | 4 |
| DOI | |
| 出版状态 | 已出版 - 2021 |
指纹
探究 'Tunable interfacial Dzyaloshinskii-Moriya interaction in symmetrical Au/[Fe/Au]:nmultilayers' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver