Ti–Zr–Cu–Co–Fe amorphous/nanocrystalline brazing filler metals for joining Ti-6Al-4V alloy

  • Rao Peng
  • , Yan Si
  • , Huyang Li
  • , Xueyin Bai
  • , Shujie Pang*
  • , Huaping Xiong
  • , Tao Zhang
  • *此作品的通讯作者
  • Beihang University
  • Beijing Institute of Aeronautical Materials

科研成果: 期刊稿件文章同行评审

摘要

A novel Ti50Zr30Cu8Co7Fe5 (at.%) amorphous/nanocrystalline brazing filler metal (BFM) with low Cu content and low liquidus temperature (1154 K) was developed and prepared into a flexible ribbon by melt-spinning for brazing Ti-6Al-4V (Ti64) alloy. The effects of vacuum brazing temperature and holding time on the microstructure and mechanical properties of the joints were investigated. For the joint brazed at a low brazing temperature of 1173 K for 15 min, a messy segregated layer consisted of α-Ti, β-Ti, and Ti2Cu intermetallic compound was formed in the center of the braze zone, resulting in relatively low tensile shear strength (~ 310 MPa) of the joint. With the brazing temperature increasing up to 1233 K, the joints exhibited uniform Widmanstätten structure mainly consisting of acicular α-Ti, β-Ti, and sporadic Ti2Cu intermetallic compound without segregated layer. The Ti64 joint brazed at 1233 K for 15 min possesses an improved tensile shear strength of ~ 400 MPa. By extending the holding time to 30 min and 45 min at the brazing temperature of 1233 K, the amount of Ti2Cu intermetallic compound in the braze zone decreased, leading to the high strength of the joints up to ~ 446 and ~ 491 MPa, respectively.

源语言英语
页(从-至)2473-2483
页数11
期刊Welding in the World, Le Soudage Dans Le Monde
68
9
DOI
出版状态已出版 - 9月 2024

学术指纹

探究 'Ti–Zr–Cu–Co–Fe amorphous/nanocrystalline brazing filler metals for joining Ti-6Al-4V alloy' 的科研主题。它们共同构成独一无二的学术指纹。

引用此