A drastic improvement in oxidation resistance of SmCo7 nanocrystalline magnet was achieved by alloying silicon at 500°C. The maximum energy product (BH) max loss of SmCo6.1 Si0.9 nanocrystalline magnet was about 5.6% after oxidation at 500°C for 500 h, which was significantly less than 52.1% of SmCo7 nanocrystalline magnet. A general mode was proposed to predict the (BH) max loss as a function of oxidation time at 500°C. The formation of SiO2 oxide in the internal oxidation layer plays an important role in reducing the oxidation rate and oxygen diffusion coefficient, which leads to the enhancement of inherent oxidation resistance of SmCo6.1 Si0.9 nanocrystalline magnet.

源语言英语
文章编号252504
期刊Applied Physics Letters
98
25
DOI
出版状态已出版 - 20 6月 2011