跳到主要导航 跳到搜索 跳到主要内容

Tensile creep behavior of three-dimensional four-step braided SiC/SiC composite at elevated temperature

  • Northwestern Polytechnical University Xian
  • Beihang University
  • China Flight Test Establishment

科研成果: 期刊稿件文章同行评审

摘要

This article presents experimental results for tensile creep deformation and rupture behavior of three-dimensional four-step braided SiC/SiC composites at 1100 °C and 1300 °C in air. The creep behavior at 1300 °C exhibited a long transient creep regime and the creep rate decreased continuously with time. The creep behavior at 1100 °C exhibited an apparent steady-rate regime and the creep deformation was smaller than that at 1300 °C. However, the creep rupture time at both temperatures showed little difference. The mechanisms controlling creep deformation and rupture behavior were analyzed.

源语言英语
页(从-至)6721-6729
页数9
期刊Ceramics International
43
9
DOI
出版状态已出版 - 15 6月 2017

指纹

探究 'Tensile creep behavior of three-dimensional four-step braided SiC/SiC composite at elevated temperature' 的科研主题。它们共同构成独一无二的指纹。

引用此