An offshore nectural gas (NG) utilization project in Bohai Bay of China is carried out and API 5L X65 steel made in China is selected for the subsea NG transmission pipeline. Whereas, H2S content in NG is increasing along with the exploitation of the field, and CO2 content is up to 10%, so the subsea pipeline faces with stress corrosion cracking risks. Therefore, on stress corrosion cracking resistance of X65 pipeline steel welded joint in simulated H2S/CO2 environment was studied by referencing the test method of NACE TM0177 - 2005. Results show that the X65 pipeline steel welded joint has excellent performance of SSCC resistance in H2S/CO2 environment. However, a certain degree of SSCC sensitivity appeared at low temperature under acidic conditions. Some suggestions for controlling SSCC were presented in order to ensure the pipeline/ s safety in running, includes controlling NG transmission temperature in a appropriate range and reducing acid gas content as far as possible.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 43-46 |
| 页数 | 4 |
| 期刊 | Corrosion and Protection |
| 卷 | 35 |
| 期 | 1 |
| 出版状态 | 已出版 - 2014 |
| 已对外发布 | 是 |
指纹
探究 'Sulfide stress corrosion cracking resistance of X65 pipeline steel welded joint in H2S/CO2 environment' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver