TY - JOUR
T1 - Stress corrosion cracking of welded API X70 pipeline steel in simulated underground water
AU - Liu, Z. Y.
AU - Du, C. W.
AU - Li, C.
AU - Wang, F. M.
AU - Li, X. G.
PY - 2013/9
Y1 - 2013/9
N2 - This paper investigates the stress corrosion cracking (SCC) behavior of welded API X70 pipeline steel in simulated underground water using the slow strain rate test, fractographic characterization by scanning electron microscopy, and potentiodynamic polarization techniques. SCC susceptibility of the heat-affected zone (HAZ) is demonstrated to be dependent on two factors: the effect of the microstructure in the HAZ on electrochemical reactions and the effect of the mechanical property on SCC occurrence. Electrochemical experiments indicate that the microstructures in the HAZ, especially the softened microstructure, can significantly facilitate the processes of hydrogen evolution when cathodic potential is positive to 21050 mVSCE. However, when the cathodic potential is below 21050 mVSCE, the cathode current densities of different microstructures are close to one another and greatly increase because of the decrease of the applied potentials. The SCC behavior is consistent with the electrochemical results. Under 2650 and 2850 mV SCE, SCC is most likely to occur in the softened region, and under 21200 mVSCE, SCC occurs in both the softened and hardened regions.
AB - This paper investigates the stress corrosion cracking (SCC) behavior of welded API X70 pipeline steel in simulated underground water using the slow strain rate test, fractographic characterization by scanning electron microscopy, and potentiodynamic polarization techniques. SCC susceptibility of the heat-affected zone (HAZ) is demonstrated to be dependent on two factors: the effect of the microstructure in the HAZ on electrochemical reactions and the effect of the mechanical property on SCC occurrence. Electrochemical experiments indicate that the microstructures in the HAZ, especially the softened microstructure, can significantly facilitate the processes of hydrogen evolution when cathodic potential is positive to 21050 mVSCE. However, when the cathodic potential is below 21050 mVSCE, the cathode current densities of different microstructures are close to one another and greatly increase because of the decrease of the applied potentials. The SCC behavior is consistent with the electrochemical results. Under 2650 and 2850 mV SCE, SCC is most likely to occur in the softened region, and under 21200 mVSCE, SCC occurs in both the softened and hardened regions.
KW - Electrochemical characteristic
KW - SCC
KW - Welding microstructure
KW - X70 pipeline steel
UR - https://www.scopus.com/pages/publications/84893689947
U2 - 10.1007/s11665-013-0575-2
DO - 10.1007/s11665-013-0575-2
M3 - 文章
AN - SCOPUS:84893689947
SN - 1059-9495
VL - 22
SP - 2550
EP - 2556
JO - Journal of Materials Engineering and Performance
JF - Journal of Materials Engineering and Performance
IS - 9