TY - JOUR
T1 - SCC evaluation of a 2297 Al-Li alloy rolled plate using the slow-strain rate technique
AU - ZHAO, Kuo
AU - LIU, Jianhua
AU - YU, Mei
AU - LI, Songmei
N1 - Publisher Copyright:
© 2019 Chinese Society of Aeronautics and Astronautics
PY - 2019/11
Y1 - 2019/11
N2 - The stress corrosion cracking (SCC) susceptibility of 2297 Al-Li alloy in 1 M NaCl + 0.01 M H2O2 solution (CP solution) and 1 M NaCl + 0.01 M H2O2 + 0.6 M Na2SO4 solution (CPS solution) was investigated by slow-strain rate tests at various strain rates ranging from 10−5 s−1 to 10−7 s−1. The roles of H2O2 and SO4 2− in the corrosion process were estimated by potentiodynamic polarization and electrochemical impedance spectroscopy. 2297 Al-Li alloy does not fracture ascribed to SCC in CP solution, while it undergoes SCC in CPS solution. In CPS solution, with a decreasing strain rate from 10−5 s−1 to 10−7 s−1, the SCC susceptibility firstly rises and then declines exhibiting a peak value at a strain rate of 10−6 s−1. H2O2 promotes the active dissolution while SO4 2− lowers the corrosion rate. The SCC fracture is associated with a decline in the dissolution rate of the crack tip by SO4 2−, which leads to stress concentration. In CPS solution, a reduction in the local dissolution rate of the crack tip leads to stress concentration, resulting in SCC fracture. As the preferred initiation site for a crack, pits also show a noteworthy effect on SCC of 2297 Al-Li alloy.
AB - The stress corrosion cracking (SCC) susceptibility of 2297 Al-Li alloy in 1 M NaCl + 0.01 M H2O2 solution (CP solution) and 1 M NaCl + 0.01 M H2O2 + 0.6 M Na2SO4 solution (CPS solution) was investigated by slow-strain rate tests at various strain rates ranging from 10−5 s−1 to 10−7 s−1. The roles of H2O2 and SO4 2− in the corrosion process were estimated by potentiodynamic polarization and electrochemical impedance spectroscopy. 2297 Al-Li alloy does not fracture ascribed to SCC in CP solution, while it undergoes SCC in CPS solution. In CPS solution, with a decreasing strain rate from 10−5 s−1 to 10−7 s−1, the SCC susceptibility firstly rises and then declines exhibiting a peak value at a strain rate of 10−6 s−1. H2O2 promotes the active dissolution while SO4 2− lowers the corrosion rate. The SCC fracture is associated with a decline in the dissolution rate of the crack tip by SO4 2−, which leads to stress concentration. In CPS solution, a reduction in the local dissolution rate of the crack tip leads to stress concentration, resulting in SCC fracture. As the preferred initiation site for a crack, pits also show a noteworthy effect on SCC of 2297 Al-Li alloy.
KW - Al-Li alloy
KW - Dissolution
KW - Electrochemical behavior
KW - Slow strain rate testing
KW - Stress corrosion cracking
UR - https://www.scopus.com/pages/publications/85062239966
U2 - 10.1016/j.cja.2019.01.022
DO - 10.1016/j.cja.2019.01.022
M3 - 文章
AN - SCOPUS:85062239966
SN - 1000-9361
VL - 32
SP - 2516
EP - 2525
JO - Chinese Journal of Aeronautics
JF - Chinese Journal of Aeronautics
IS - 11
ER -