Pitting corrosion of X70 pipeline steel in the simulated wet storage environment

  • Zhiyong Liu
  • , Chaofang Dong
  • , Zhijun Jia
  • , Xiaogang Li*
  • *此作品的通讯作者
  • University of Science and Technology Beijing
  • Nanchang Hangkong University

科研成果: 期刊稿件文章同行评审

摘要

Pitting mechanism and behaviour of X70 pipeline steel in humid storage environments were investigated using electrochemical polarization curves, electrochemical impedance spectrums (EIS), immersing corrosion tests and corrosion morphology observation through SEM. It was demonstrated that pitting of X70 pipeline steel occurred in simulated moist storage environments, for which the corrosive substances came from the residual species in laminar cooling water introduced during steel manufacture processes. HCO3- and NO3- are passivating agents, Cl- and SO42- would destroyed the passivation layer, which could lead to pitting. In solution with 0.5 mol/L NaHCO3, 0.02 mol/L Cl- was enough to break the passivation layer. Cl- concentration is a key factor for pitting initiation and propagation. When the Cl- concentration was relatively low, pitting could initiate but was hard to grow up. When the Cl- concentration was moderate (about 0.149 mol/L), pitting sensitivity was the highest because pitting was easy to grow up. However, if the concentration of Cl- was too high, uniform corrosion occurred.

源语言英语
页(从-至)1009-1016
页数8
期刊Jinshu Xuebao/Acta Metallurgica Sinica
47
8
DOI
出版状态已出版 - 8月 2011