Diffusion bonding of TC4 and QAL10-3-1. 5 was carried out under the condition of 850 ° , 8 MPa and 30 min, but there are cracks existing on local area of diffusion zone. Microstructure of diffusion zone was analyzed using scanning electron microscopy ( SEM) , and diffusion distance and concentration distribution of elements were analyzed using EDS. The result shows that the transition zone thickness is 10 μm. Diffusion distance of element increases with increasing bonding time followed a parabolic law; x2 = Kp (t - t0) , and phenomenon of transition zone moving to TC4 are observed which is so called kirkendall effect . The occurrence of the cracks on the diffusion zone was studied in the theory of interfacial pore and the reason for micro-cracks produced and improvement methods are found out. Thus, approving diffusion joint is attained by improving the welding process.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 285-288 |
| 页数 | 4 |
| 期刊 | Jilin Daxue Xuebao (Gongxueban)/Journal of Jilin University (Engineering and Technology Edition) |
| 卷 | 36 |
| 期 | 3 |
| 出版状态 | 已出版 - 5月 2006 |
| 已对外发布 | 是 |
学术指纹
探究 'Pattern analysis on diffusion bonding of TC4 and QAL10-3-1.5' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver