TY - JOUR
T1 - Mxene-toughened Al2O3 ceramic at high temperature
AU - Liang, Lei
AU - Sun, Xianxian
AU - Ning, Yuanhao
AU - Wang, Shasha
AU - Yin, Weilong
AU - Li, Yibin
N1 - Publisher Copyright:
© 2023 Elsevier Ltd
PY - 2023/11
Y1 - 2023/11
N2 - The process of toughening brittle ceramics is challenging but important for broadening their range of applications. Extensive studies on toughening brittle alumina (Al2O3) ceramics at room temperature have been conducted; however, significantly increasing their toughness at high temperatures remains a challenge. Here, we propose the use of two-dimensional Ti3C2Tx MXene ceramics with high thermal stability to effectively toughen Al2O3 ceramics at high temperatures via a nacre-like structure strategy. The fracture toughness (KJc) of the as-prepared MXene/Al2O3 nanocomposite at 1000 °C is 6.02 MPa m1/2, 2.4 times that of pure Al2O3 (2.51 MPa m1/2). Moreover, it maintains relatively high strength at 1000 °C (∼193 MPa). The toughening mechanisms - crack deflection, bifurcation and bridging effects - are obtained via in situ observation of crack propagation and finite element simulation. Our novel strategy provides a universal solution to improve the toughness of brittle ceramics at high temperatures and in some special environments.
AB - The process of toughening brittle ceramics is challenging but important for broadening their range of applications. Extensive studies on toughening brittle alumina (Al2O3) ceramics at room temperature have been conducted; however, significantly increasing their toughness at high temperatures remains a challenge. Here, we propose the use of two-dimensional Ti3C2Tx MXene ceramics with high thermal stability to effectively toughen Al2O3 ceramics at high temperatures via a nacre-like structure strategy. The fracture toughness (KJc) of the as-prepared MXene/Al2O3 nanocomposite at 1000 °C is 6.02 MPa m1/2, 2.4 times that of pure Al2O3 (2.51 MPa m1/2). Moreover, it maintains relatively high strength at 1000 °C (∼193 MPa). The toughening mechanisms - crack deflection, bifurcation and bridging effects - are obtained via in situ observation of crack propagation and finite element simulation. Our novel strategy provides a universal solution to improve the toughness of brittle ceramics at high temperatures and in some special environments.
KW - A. Layered structures
KW - B. Fracture toughness
KW - B. High-temperature properties
KW - TiCT MXene
UR - https://www.scopus.com/pages/publications/85168132679
U2 - 10.1016/j.compositesa.2023.107714
DO - 10.1016/j.compositesa.2023.107714
M3 - 文章
AN - SCOPUS:85168132679
SN - 1359-835X
VL - 174
JO - Composites Part A: Applied Science and Manufacturing
JF - Composites Part A: Applied Science and Manufacturing
M1 - 107714
ER -