摘要
Abstract Cyclic thermal exposure tests of infrared heating to 800 °C in 120 s followed by compressed air cooling to 150 °C in 60 s were performed for the laser deposited Ti60A (Ti5.54Al3.38Sn3.34Zr0.37Mo0.46Si) alloy. The effects of thermal exposure cycles on length of β phase, area fraction of α phase and microhardness of alloy were examined by OM, SEM and EDS. The results indicate that thermal exposure cycles have significant effects on length of β phase, area fraction of α phase and microhardness of the alloy. The original fine basket-weave β and 78.5% α transform to transient wedge-like β, finally leaving granular β and 97.6% coarsened α with the increased thermal exposure cycles. The formation mechanism of coarsened α and broken-up β microstructure is discussed. The alloy after 750 thermal exposure cycles has the maximum microhardness, 33.3% higher than that of the as-deposited alloy.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 3249-3256 |
| 页数 | 8 |
| 期刊 | Transactions of Nonferrous Metals Society of China (English Edition) |
| 卷 | 23 |
| 期 | 11 |
| DOI | |
| 出版状态 | 已出版 - 11月 2013 |
指纹
探究 'Microstructure evolution of laser deposited Ti60A titanium alloy during cyclic thermal exposure' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver