Wear resistant Cr-Cu-Si metal silicide alloys with different Cu contents were fabricated by the laser melting process. The Cr-Cu-Si alloys have a similar microstructure consisting of the Cr5Si3/CrSi dual-phase primary dendrites and the interdendritic Cu-based solid solution (Cuss). The Cu content has no effect on the phase constitutions of the alloys. The Cr5Si3/CrSi dendrite volume fraction and hardness of the Cr-Cu-Si alloys decrease with the increasing Cu content. Wear test results indicate that all the Cuss-toughened metal silicide alloys have excellent wear resistance and low coefficient of friction. Wear resistance increases and friction coefficient decreases with the decreasing Cu content.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 218-224 |
| 页数 | 7 |
| 期刊 | Journal of Alloys and Compounds |
| 卷 | 420 |
| 期 | 1-2 |
| DOI | |
| 出版状态 | 已出版 - 31 8月 2006 |
学术指纹
探究 'Microstructure and tribological properties of Cuss-toughened Cr-Cu-Si metal silicide alloys' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver