TY - JOUR
T1 - Microstructural evolution and mechanical properties of an Nb-16Si in-situ composite with Fe additions prepared by arc-melting
AU - Zhou, J. R.
AU - Sha, J. B.
N1 - Publisher Copyright:
© 2012 Elsevier Ltd. All rights reserved.
PY - 2013/3
Y1 - 2013/3
N2 - This paper deals with phase constitutions, microstructural evolutions, and mechanical properties of Nb-16Si-xFe in-situ composites (where x = 2, 4, 6 at.%, referred as to 2Fe, 4Fe and 6Fe alloys, hereafter) prepared by arc-melting. It is found that with additions of Fe, Nb4FeSi silicide arises and microstructures of as-cast samples are consisted of dendritic-like NbSS phase, Nb3Si block, and Nb4FeSi matrix in the 2Fe and 4Fe alloys, and of the dendritic-like NbSS phase and Nb4FeSi matrix in the 6Fe alloy. When heat-treated at 1350°C for 100 h, part of the Nb3Si phase decomposes in the 2Fe and 4Fe alloys, and the 6Fe alloy shows no change in microstructure as compared with the as-cast one. The Nb4FeSi silicide is found to be brittle, its fracture toughness and elastic modulus are first obtained, having values about 1.22 MPa m1/2, and 310 GPa, respectively. The fracture toughness of the bulk as-cast and heat-treated Nb-16Si-xFe samples are changed slightly by the Fe additions, which is in a range of 9.03-10.19 MPa m1/2. It is interesting that at room temperature, strength is improved by the Fe additions, whereas at 1250°C and 1350°C the strength decreases. As the Fe content increased from 2 at.% to 6 at.%, for example, the 0.2% yield strength increases from 1410 MPa to 1580 MPa at room temperature, decreases from 479 MPa to 385 MPa at 1250°C.
AB - This paper deals with phase constitutions, microstructural evolutions, and mechanical properties of Nb-16Si-xFe in-situ composites (where x = 2, 4, 6 at.%, referred as to 2Fe, 4Fe and 6Fe alloys, hereafter) prepared by arc-melting. It is found that with additions of Fe, Nb4FeSi silicide arises and microstructures of as-cast samples are consisted of dendritic-like NbSS phase, Nb3Si block, and Nb4FeSi matrix in the 2Fe and 4Fe alloys, and of the dendritic-like NbSS phase and Nb4FeSi matrix in the 6Fe alloy. When heat-treated at 1350°C for 100 h, part of the Nb3Si phase decomposes in the 2Fe and 4Fe alloys, and the 6Fe alloy shows no change in microstructure as compared with the as-cast one. The Nb4FeSi silicide is found to be brittle, its fracture toughness and elastic modulus are first obtained, having values about 1.22 MPa m1/2, and 310 GPa, respectively. The fracture toughness of the bulk as-cast and heat-treated Nb-16Si-xFe samples are changed slightly by the Fe additions, which is in a range of 9.03-10.19 MPa m1/2. It is interesting that at room temperature, strength is improved by the Fe additions, whereas at 1250°C and 1350°C the strength decreases. As the Fe content increased from 2 at.% to 6 at.%, for example, the 0.2% yield strength increases from 1410 MPa to 1580 MPa at room temperature, decreases from 479 MPa to 385 MPa at 1250°C.
KW - A. Intermetallics
KW - A. Ternary alloy system
KW - B. Phase identification
KW - D. Microstructure
KW - E. Mechanical properties
UR - https://www.scopus.com/pages/publications/84869886440
U2 - 10.1016/j.intermet.2012.10.017
DO - 10.1016/j.intermet.2012.10.017
M3 - 文章
AN - SCOPUS:84869886440
SN - 0966-9795
VL - 34
SP - 1
EP - 9
JO - Intermetallics
JF - Intermetallics
ER -