TY - JOUR
T1 - Microstructural changes of a creep-damaged nickel-based K002 superalloy containing hf element under different HIP temperatures
AU - Wang, Xiaomeng
AU - Zhou, Yu
AU - Dong, Jian
AU - Wang, Tianyou
AU - Zhao, Zihua
AU - Zhang, Zheng
N1 - Publisher Copyright:
© 2016 by De Gruyter.
PY - 2016/2/1
Y1 - 2016/2/1
N2 - Effects of hot isostatic pressing (HIP) temperature on the microstructural evolution of a nickel-based K002 superalloy containing Hf element after long-term service were investigated using three different soaking temperatures during HIP. The degraded γ′ precipitates represented coarse and irregular morphology after long-term service. These γ′ precipitates still were of coarse and irregular shape, but the size and volume fraction of γ′ precipitates were markedly reduced under HIP condition of 1,190°C/200 MPa/4 h, indicating that the γ′ precipitates were experiencing a dissolution process. Meanwhile, the concentrically oriented N-type γ′ rafting structure around the cavities was formed. With HIP temperature increase to 1,220°C and 1,250°C, the small-sized, cubic and regular γ′ precipitates were re-precipitated, and the concentrically oriented γ′ structure vanished. The unstable morphology induced by the nucleation and growth of γ matrix was found near the creep cavities, indicating that the solute atoms diffused inward the creep-induced cavities during HIP. However, at HIP temperature of 1,220°C and 1,250°C, a large number of blocky MC(2)-type carbides containing amounts of Hf elements were precipitated, demonstrating that HIP treatment at higher temperatures can result in the formation of a large number of blocky MC(2)-type carbides.
AB - Effects of hot isostatic pressing (HIP) temperature on the microstructural evolution of a nickel-based K002 superalloy containing Hf element after long-term service were investigated using three different soaking temperatures during HIP. The degraded γ′ precipitates represented coarse and irregular morphology after long-term service. These γ′ precipitates still were of coarse and irregular shape, but the size and volume fraction of γ′ precipitates were markedly reduced under HIP condition of 1,190°C/200 MPa/4 h, indicating that the γ′ precipitates were experiencing a dissolution process. Meanwhile, the concentrically oriented N-type γ′ rafting structure around the cavities was formed. With HIP temperature increase to 1,220°C and 1,250°C, the small-sized, cubic and regular γ′ precipitates were re-precipitated, and the concentrically oriented γ′ structure vanished. The unstable morphology induced by the nucleation and growth of γ matrix was found near the creep cavities, indicating that the solute atoms diffused inward the creep-induced cavities during HIP. However, at HIP temperature of 1,220°C and 1,250°C, a large number of blocky MC(2)-type carbides containing amounts of Hf elements were precipitated, demonstrating that HIP treatment at higher temperatures can result in the formation of a large number of blocky MC(2)-type carbides.
KW - HIP
KW - diffusion
KW - microstructure
KW - rafting
UR - https://www.scopus.com/pages/publications/84958180545
U2 - 10.1515/htmp-2014-0128
DO - 10.1515/htmp-2014-0128
M3 - 文章
AN - SCOPUS:84958180545
SN - 0334-6455
VL - 35
SP - 153
EP - 159
JO - High Temperature Materials and Processes
JF - High Temperature Materials and Processes
IS - 2
ER -