Joining of SiC ceramic to Ni-based superalloy with functionally gradient material fillers and a tungsten intermediate layer

  • Shujie Li*
  • , Ying Zhou
  • , Huiping Duan
  • , Jianhui Qiu
  • , Yan Zhang
  • *此作品的通讯作者
  • Beihang University
  • Akita Prefectural University
  • University of Science and Technology Beijing

科研成果: 期刊稿件文章同行评审

摘要

Joining of ceramics to metals is of great interest from both technical and economical points of view. SHS welding of SiC ceramic to Ni-based superalloy has been achieved with TiC-Ni functionally gradient materials as filler and a tungsten sheet as an intermediate layer. The obtained welded strength of the welded sample is 60% of the strength of the SiC ceramic measured under the identical conditions. This value is 25% greater than that without the tungsten intermediate layer. Within the range tested in this study, the strength of welded samples increases with increasing thickness of the tungsten layer. The presence of the tungsten intermediate layer can effectively improve the distribution of process-induced thermal stresses in the joints and reduce the concentration of residual thermal stresses in the ceramic near the welding seam. Microstructural study reveals that diffusion takes place at the interfaces, which promotes bonding at the interfaces.

源语言英语
页(从-至)4065-4070
页数6
期刊Journal of Materials Science
38
19
DOI
出版状态已出版 - 1 10月 2003

学术指纹

探究 'Joining of SiC ceramic to Ni-based superalloy with functionally gradient material fillers and a tungsten intermediate layer' 的科研主题。它们共同构成独一无二的学术指纹。

引用此