摘要
In this paper, 'in-situ' weld-alloying/laser beam welding with titanium as alloying element is utlized to join SiCp/6061 Al MMC in order to prevent the formation of the needle-like harmful Al4C3 phases in the weld. Microstructure of the weld is characterized as functions of alloying content and processing parameters. Results show that the needle-like harmful aluminum carbides are completely eliminated. A central fusion weld joint reinforced by TiC, Ti5Si3 and Al3Ti is produced by 'in-situ' weld-alloying/laser beam welding of SiCp/6061 Al MMC, while some large pores are formed in the partly melted zone. (C) 2000 Elsevier Science S.A. All rights reserved.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 1-6 |
| 页数 | 6 |
| 期刊 | Materials Science and Engineering: A |
| 卷 | 293 |
| 期 | 1-2 |
| DOI | |
| 出版状态 | 已出版 - 2000 |