摘要
Abstract: Mo–Si–B alloys were obtained by spark plasma sintering (SPS) using fine Mo–Si–B alloy powders with a particle size of 2.5 μm. The SPS Mo–Si–B alloys consisted of fine MoSi2/Mo2Bi5(Mo5Si3)/MoB/SiO2 phases. Under isothermal conditions, the weight-gain kinetics of the Mo–Si–B alloys obtained by SPS exhibited parabolic time dependence and these Mo–Si–B alloys showed better oxidation resistance at moderate temperatures of 500 °C and 600 °C with no “pest” failure. The oxide scale on the sample surface consisted of MoO3, amorphous borosilicate and crystalloid SiO2 phases. An increase in the oxidation temperature from 500 to 600 °C caused a significantly higher fluidity and a shorter incubation stage for the formation of a continuously protective borosilicate layer, so that the mass gain was smaller than 1 mg/cm2 for oxidation at 600 °C for 100 h, which corresponds to the excellent oxidation resistance. Graphic Abstract: [Figure not available: see fulltext.].
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 243-257 |
| 页数 | 15 |
| 期刊 | Oxidation of Metals |
| 卷 | 92 |
| 期 | 3-4 |
| DOI | |
| 出版状态 | 已出版 - 1 10月 2019 |
指纹
探究 'Improvement of “Pest” Resistance of MoSi2 Intermetallic Compound at 500 °C and 600 °C via Addition of B Fabricated by Spark Plasma Sintering' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver