Improvement in interlaminar strength and galvanic corrosion resistance of CFRP/Mg laminates by laser ablation

  • Yingcai Pan
  • , Guoqing Wu*
  • , Zheng Huang
  • , Zongke Zhang
  • , Hengjian Ye
  • , Maoyuan Li
  • , Sudong Ji
  • *此作品的通讯作者
  • Beihang University
  • CAS - Institute of Mechanics

科研成果: 期刊稿件文章同行评审

摘要

In this study, the magnesium alloy sheet was treated by laser ablation to develop a type of conversion film on magnesium alloy aimed for simultaneous improvement in interlaminar strength and galvanic corrosion resistance of CFRP/Mg laminates. The results show that laser ablation can effectively enhance the Mode I (peel) interlaminar strength of CFRP/Mg laminates due to the formation of chaotic structure on the magnesium surface, and the peel strength decreases with the increase of scan speed. In addition, the laser ablation layer can provide an excellent protection against the galvanic corrosion in CFRP/Mg laminates, since the isolation between carbon fibre and magnesium substrate can be obtained by laser ablation.

源语言英语
页(从-至)4-7
页数4
期刊Materials Letters
207
DOI
出版状态已出版 - 15 11月 2017

指纹

探究 'Improvement in interlaminar strength and galvanic corrosion resistance of CFRP/Mg laminates by laser ablation' 的科研主题。它们共同构成独一无二的指纹。

引用此