High mobility 2-dimensional electron gas at LaAlO3/SrTiO3 interface prepared by spin coating chemical methods

  • Tahira Khan
  • , Hui Zhang
  • , Hongrui Zhang
  • , Xi Yan
  • , Deshun Hong
  • , Furong Han
  • , Yuansha Chen
  • , Baogen Shen
  • , Jirong Sun
  • CAS - Institute of Physics
  • Chinese Academy of Sciences

科研成果: 期刊稿件文章同行评审

摘要

Highly mobile 2-dimensional electron gases (2DEGs) at the (001), (011) and (111)-oriented LaAlO3/SrTiO3 (LAO/STO) interfaces are obtained using spin coating chemical method, which is a gentle technique without plasma bombardment of the pulsed laser deposition. As revealed by x-ray diffraction spectrum and x-ray reflectivity analysis, the LAO over layer is epitaxially grown, and has a uniform thickness of ∼15 nm, ∼20 nm and ∼26 nm for (001), (011) and (111) orientations, respectively. The interfaces are well metallic down to 2 K. The carrier mobilities are ∼28 000 cm2 V-1 s-1, ∼22 000 cm2 V-1 s-1 and ∼8300 cm2 V-1 s-1 at 2 K for the (001), (011) and (111) LAO/STO interfaces, respectively, and ∼8 cm2 V-1 s-1, ∼4 cm2 V-1 s-1 and ∼4 cm2 V-1 s-1 at room temperature. The present work shows that the spin coating chemical method is a feasible approach to get high quality 2DEG at both the polar/non-polar and polar/polar interfaces.

源语言英语
文章编号435701
期刊Nanotechnology
28
43
DOI
出版状态已出版 - 26 9月 2017
已对外发布

指纹

探究 'High mobility 2-dimensional electron gas at LaAlO3/SrTiO3 interface prepared by spin coating chemical methods' 的科研主题。它们共同构成独一无二的指纹。

引用此