Galvanic Corrosion Behavior of 6082 Aluminum Alloy Coupled to SUS304 in Simulated Water Circumstance with Various Salt Concentrations

  • Chongqing Institute of Technology

科研成果: 期刊稿件文章同行评审

摘要

The galvanic corrosion behavior of 6082 aluminum alloy coupled to SUS304 was assessed in various NaCl solutions to simulate the various salt water environments. Results showed that the 6082/SUS304 couple was composed of macro-couple (6082/SUS304) and micro-couple (Mg2Si or Al(Mn, Fe, Cr, Cu) Si coupled to α-Al), and the galvanic corrosion process intensified with the increased NaCl concentration, especially the Mg2Si micro-couple experienced a polarity reversal. The erosive effect of Cl induced the corrosion products to exhibit an evolution tendency of “Al2O3 → Al(OH)3 → Al(OH)3−xClx → AlCl3”. Furthermore, the distributions of potential and current susceptible to the 6082/SUS304 structure were simulated by COMSOL (FEM) and the mechanisms were discussed.

源语言英语
页(从-至)29981-29997
页数17
期刊Journal of Materials Engineering and Performance
35
29
DOI
出版状态已出版 - 8月 2026

学术指纹

探究 'Galvanic Corrosion Behavior of 6082 Aluminum Alloy Coupled to SUS304 in Simulated Water Circumstance with Various Salt Concentrations' 的科研主题。它们共同构成独一无二的学术指纹。

引用此