Fatigue behavior of welded joints of a Ni–Fe-based superalloy

  • Beihang University
  • Beijing Key Laboratory of Aero-Engine Structure and Strength

科研成果: 期刊稿件文章同行评审

摘要

This study investigated the fatigue behavior of butt weld joints in a Ni–Fe-based superalloy GH1140 at 650 °C. The welded joints were prepared by the gas tungsten arc welding process on GH1140 plates with a thickness of 20 mm and a 45° K-shape groove. Vickers hardness tests on the cross-section of the welded joints showed slightly lower hardness in the weld center compared to the base metal. Fatigue test results demonstrated a reduction in fatigue lifetime for the welded joints compared to the base metal, attributable to the combined effects of reduced hardness in the weld metal and material heterogeneity. The reduction in lifetime was found to be stress-dependent, with a transition from fatigue fracture at lower stress levels to shear fracture at higher stress levels. Moreover, an empirical fatigue lifetime prediction model was used to predict the fatigue lifetime of the welded joints, showing good agreement with experimental data.

源语言英语
页(从-至)657-669
页数13
期刊Welding in the World, Le Soudage Dans Le Monde
69
3
DOI
出版状态已出版 - 3月 2025

指纹

探究 'Fatigue behavior of welded joints of a Ni–Fe-based superalloy' 的科研主题。它们共同构成独一无二的指纹。

引用此