Fabrication of single-crystal superalloy hollow blade based on integral ceramic mold

  • Wenliang Xu
  • , Zhongliang Lu*
  • , Guoqiang Tian
  • , Kai Miao
  • , Dichen Li
  • , Weijun Zhu
  • , Fu Wang
  • , Hang Zhang
  • , Yong Wang
  • , Yang Song
  • *此作品的通讯作者
  • Xi'an Jiaotong University
  • Collaborative Innovation Center for Advanced Aero-Engine
  • Zhengzhou University of Aeronautics
  • Chengdu Aerospace Superalloy Technology Co., Ltd.

科研成果: 期刊稿件文章同行评审

摘要

The integral ceramic mold technique based on stereolithography additive manufacturing and gelcasting technology was applied to casting single-crystal (SX) superalloy parts. The fabrication process for producing alumina-based ceramic molds with kyanite additive and the resultant mold structures were investigated. The results showed that the fabricated alumina-based molds exhibited superior high-temperature mechanical performance and dimensional stability. The high-temperature mechanical performance was attributed to the addition of suitable amounts of kyanite, which led to the mullitization of the raw materials. Moreover, the volume expansion that accompanied kyanite decomposition enabled well-controlled sintering shrinkage and apparent porosity. The ceramic molds prepared with the optimal amount of kyanite exhibited favorable bending strength, creep deformation, sintering shrinkage, and apparent porosity for directional solidification of SX superalloys. Cast trials of a hollow turbine blade using CMSX-4 SX superalloy demonstrated the potential of the proposed approach for rapid-cast SX superalloy parts.

源语言英语
页(从-至)615-622
页数8
期刊Journal of Materials Processing Technology
271
DOI
出版状态已出版 - 9月 2019
已对外发布

指纹

探究 'Fabrication of single-crystal superalloy hollow blade based on integral ceramic mold' 的科研主题。它们共同构成独一无二的指纹。

引用此