摘要
Pure CeO 2 and La doped CeO 2 (LDC) coatings were prepared on nickel-based substrates by electron beam physical vapor deposition at 1173 K. The infrared emissivity in 2.5-25 μm of LDC coatings was enhanced with the increase of La concentration at high temperature 873-1273 K. Compared to the undoped CeO 2 coating, the infrared emissivity of 16.7% LDC coating increases by 55%, and reaches up to 0.9 at 873 K. The enhancement of doped coatings' emissivity is attributed to the increasing lattice absorption and free-carrier absorption. The high emissivity LDC coatings show a promising potential in high temperature application.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 605-609 |
| 页数 | 5 |
| 期刊 | Applied Surface Science |
| 卷 | 280 |
| DOI | |
| 出版状态 | 已出版 - 1 9月 2013 |
| 已对外发布 | 是 |