Effects of Nb on stress corrosion cracking of high-strength low-alloy steel in simulated seawater

  • Qianqian Qiao
  • , Lin Lu
  • , Endian Fan
  • , Jinbin Zhao
  • , Yanning Liu
  • , Guangchun Peng
  • , Yunhua Huang*
  • , Xiaogang Li
  • *此作品的通讯作者
  • University of Science and Technology Beijing
  • Nanjing Iron & Steel Co., Ltd.

科研成果: 期刊稿件文章同行评审

摘要

In this study, simulated heat-affected zone (HAZ) of Nb-free and Nb-bearing steel were obtained, and SEM, TEM, and slow strain rate tensile (SSRT) tests were performed to investigate the effect of Nb on the stress corrosion cracking (SCC) behavior of high-strength low-alloy (HLSA) steel in simulated seawater with or without hydrogen charging. The addition of Nb significantly refined the grains and uniformed the microstructure of HLSA. Nb hardly affected the SCC susceptibility of BM and HAZ without hydrogen-charging. However, after charging with 10 mA cm−2, the SCC resistance of Nb-bearing steel, especially the coarse grain HAZ (CGHAZ) improved drastically, and the process of crack initiation and propagation was inhibited owing to the hydrogen trap function of NbC precipitates.

源语言英语
页(从-至)27962-27973
页数12
期刊International Journal of Hydrogen Energy
44
51
DOI
出版状态已出版 - 22 10月 2019
已对外发布

联合国可持续发展目标

此成果有助于实现下列可持续发展目标:

  1. 可持续发展目标 7 - 经济适用的清洁能源
    可持续发展目标 7 经济适用的清洁能源

学术指纹

探究 'Effects of Nb on stress corrosion cracking of high-strength low-alloy steel in simulated seawater' 的科研主题。它们共同构成独一无二的学术指纹。

引用此