摘要
The electrochemical corrosion behavior of 20#carbon steel in NACE solutions containing different mass concentrations of H2S (0, 95.61, 103.22, and 224.16 mg·L-1 ) at different temperatures (25, 35, and 45°C) was investigated by potentiodynamic polarization tests, electrochemical impedance spectroscopy (EIS), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS). The formation mechanism of corrosion products was also discussed. It is found that the corrosion rate of the carbon steel increases significantly with the addition of a small amount of H2S in the NACE solution by promoting both the anodic iron dissolution and the cathodic hydrogen evolution. The corrosion current density of the carbon steel enhances with the increment of H2S concen-tration. As the temperature of the electrolyte solution increasing, the corrosion rate also increases. The outer loose corrosion products are mainly iron carbonate; but corrosion products formed on the steel surface are mainly composed of iron sulfides.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 1152-1158 |
| 页数 | 7 |
| 期刊 | Beijing Keji Daxue Xuebao/Journal of University of Science and Technology Beijing |
| 卷 | 34 |
| 期 | 10 |
| 出版状态 | 已出版 - 10月 2012 |
指纹
探究 'Effect of H2S concentration and temperature on the corrosion behavior of carbon steel in NACE solution' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver