TY - JOUR
T1 - Effect of doping Mg on the microstructure and mechanical behaviours of a novel Co-9Al-4.5W-4.5Mo-2Ta-0.02B alloy at room- and high-temperatures
AU - Guo, Yijia
AU - Zhong, Fei
AU - Yu, Youxing
AU - Li, Shusuo
AU - Sha, Jiangbo
N1 - Publisher Copyright:
© 2017 Elsevier B.V.
PY - 2017
Y1 - 2017
N2 - The microstructure and mechanical behaviour of a novel magnesium (Mg) doped Co-9Al-4.5W-4.5Mo-2Ta-0.02B alloy (doped 0.1, 0.3, 0.7 and 1.0 at.% Mg, referred to as 0.1Mg, 0.3Mg, 0.7Mg and 1Mg alloys hereafter, respectively) at room- and high- temperatures have been investigated. All alloys aged at 800 °C for 50 h consist of a Co solid-solution matrix (γ-CoSS) and nano-scale cuboidal γ′-Co3(Al, W) precipitates. Mg is observed to segregate primarily at the grain boundaries and the γ′-Co3(Al, W) phase. In the 0.7Mg and 1Mg alloys more Mg segregation at the grain boundaries decreases the fraction of Σ1∼3 type grain boundaries and the capability of excluding impurity O from the grain boundaries. With decreased Σ1∼3 boundaries and higher O content, the 0.7Mg and 1Mg alloys fracture in a mixed transgranular-intergranular mode at room temperature with lower strength and ductility under tension. However, the 0.1 and 0.3Mg alloys fracture in a transgranular mode with higher strength and ductility. The four alloys exhibit compressive flow stress anomalies at 700 °C and the strength obviously decreases when the nominal Mg contents increase to 0.7–1 at.% at 600–800 °C. As for the 0.1Mg and 0.3Mg alloys, the strengths from room temperature to 800 °C are higher and not obviously affected by the nominal Mg contents, primarily owing to the two alloys having almost the same and higher Σ1∼3 grain boundary fraction and the lower O concentration in the grain boundary.
AB - The microstructure and mechanical behaviour of a novel magnesium (Mg) doped Co-9Al-4.5W-4.5Mo-2Ta-0.02B alloy (doped 0.1, 0.3, 0.7 and 1.0 at.% Mg, referred to as 0.1Mg, 0.3Mg, 0.7Mg and 1Mg alloys hereafter, respectively) at room- and high- temperatures have been investigated. All alloys aged at 800 °C for 50 h consist of a Co solid-solution matrix (γ-CoSS) and nano-scale cuboidal γ′-Co3(Al, W) precipitates. Mg is observed to segregate primarily at the grain boundaries and the γ′-Co3(Al, W) phase. In the 0.7Mg and 1Mg alloys more Mg segregation at the grain boundaries decreases the fraction of Σ1∼3 type grain boundaries and the capability of excluding impurity O from the grain boundaries. With decreased Σ1∼3 boundaries and higher O content, the 0.7Mg and 1Mg alloys fracture in a mixed transgranular-intergranular mode at room temperature with lower strength and ductility under tension. However, the 0.1 and 0.3Mg alloys fracture in a transgranular mode with higher strength and ductility. The four alloys exhibit compressive flow stress anomalies at 700 °C and the strength obviously decreases when the nominal Mg contents increase to 0.7–1 at.% at 600–800 °C. As for the 0.1Mg and 0.3Mg alloys, the strengths from room temperature to 800 °C are higher and not obviously affected by the nominal Mg contents, primarily owing to the two alloys having almost the same and higher Σ1∼3 grain boundary fraction and the lower O concentration in the grain boundary.
KW - Co-Al-W based alloys
KW - Grain boundary
KW - Intermetallics
KW - Mechanical properties
KW - Microstructure
KW - Precipitation
UR - https://www.scopus.com/pages/publications/85016456943
U2 - 10.1016/j.jallcom.2017.03.259
DO - 10.1016/j.jallcom.2017.03.259
M3 - 文章
AN - SCOPUS:85016456943
SN - 0925-8388
VL - 710
SP - 725
EP - 735
JO - Journal of Alloys and Compounds
JF - Journal of Alloys and Compounds
ER -