跳到主要导航 跳到搜索 跳到主要内容

Creep Analysis of DZ411 Directionally Solidified Superalloys with APS Thermal Barrier Coating

  • Karkash Alynur
  • , Zhikun Li
  • , Chenhong Du
  • , Shun Yang*
  • *此作品的通讯作者
  • Beihang University
  • Xi'an Jiaotong University
  • Dalian University of Technology
  • CAS - Shanghai Institute of Ceramics

科研成果: 书/报告/会议事项章节 › 会议稿件 › 同行评审

摘要

With the continuous increase in turbine inlet temperature of ground-based gas turbines, research into the creep behavior of high-temperature alloys and their thermal barrier coating systems in extreme service environments has become key to ensuring long component life and reliability. This study systematically analyzes the creep deformation of directionally solidified nickel-based superalloy DZ411 and its APS thermal barrier coating and compares it with experimental data. This study primarily establishes a solid cylinder model of the coating-substrate system, employing different creep models for different layers, achieving detailed characterization of the entire creep stage of the substrate and the primary and secondary creep stages of the APS thermal barrier coating, and combines it with finite element method for numerical simulation calculations to verify the applicability of the model under complex thermo-mechanical coupling and the creep deformation behavior.

源语言英语
主期刊名Proceedings of the 6th Chinese National Congress on Thermal Stresses NCTS 2025
编辑Yu’e Ma, Xudan Yao, Wandong Wang, Cunfa Gao, Ji Wang, Yuanye Liu
出版商Springer Science and Business Media Deutschland GmbH
页157-166
页数10
ISBN(印刷版)9789819526314
DOI
出版状态已出版 - 2025
活动6th Chinese National Congress on Thermal Stresses, NCTS 2025 - Xi’an, 中国
期限: 18 4月 2025 → 20 4月 2025

丛书

姓名Springer Proceedings in Physics
卷326 SPPHY
ISSN(印刷版)0930-8989
ISSN(电子版)1867-4941

会议

会议6th Chinese National Congress on Thermal Stresses, NCTS 2025
国家/地区中国
市Xi’an
时期18/04/25 → 20/04/25

学术指纹

探究 'Creep Analysis of DZ411 Directionally Solidified Superalloys with APS Thermal Barrier Coating' 的科研主题。它们共同构成独一无二的学术指纹。

引用此