TY - JOUR
T1 - Continuous protective layer derived from organic-inorganic hybrid particles
T2 - An effective method for thermal degradation resistance and mechanical performance of phthalonitrile composites
AU - Fan, Haizhou
AU - Ren, Zhiyi
AU - Zuo, Xiaobiao
AU - Sun, Baogang
AU - Guo, Ying
AU - Li, Min
AU - Zhou, Heng
AU - Zhao, Tong
N1 - Publisher Copyright:
© 2025
PY - 2025/2
Y1 - 2025/2
N2 - In order to meet the aerospace applications, a series organic-inorganic hybrid particles (PEB1-3) were prepared by coating polyetherketone-cardo (PEK-C) on the boron powders to improve the thermal degradation resistance of phthalonitrile (PN). A continuous protective layer derived from hybrid particles can form at high temperatures, effectively isolating heat and oxygen. After adding 22.5 wt% PEB2, the temperature of 5 % mass loss (T5%) of PN hybrid resin (PN-PEB2) was significantly delayed from 485 °C to 535 °C. PEB2 exhibited outstanding heat-resistant modification efficiency in PN matrix. In a series of thermal degradation experiments, the surface morphology of PN-PEB2 was mostly maintained after thermal degradation at decomposition temperature. For PN-PEB2 composite, the flexural strength (FS) and interlaminar shear strength (ILSS) were increased by 40.4 % and 44.8 % compared with the PN composite, respectively. After thermal degradation at 350 °C for 100 h, the FS retention rate of PN-PEB2 composite was 67.1 %.
AB - In order to meet the aerospace applications, a series organic-inorganic hybrid particles (PEB1-3) were prepared by coating polyetherketone-cardo (PEK-C) on the boron powders to improve the thermal degradation resistance of phthalonitrile (PN). A continuous protective layer derived from hybrid particles can form at high temperatures, effectively isolating heat and oxygen. After adding 22.5 wt% PEB2, the temperature of 5 % mass loss (T5%) of PN hybrid resin (PN-PEB2) was significantly delayed from 485 °C to 535 °C. PEB2 exhibited outstanding heat-resistant modification efficiency in PN matrix. In a series of thermal degradation experiments, the surface morphology of PN-PEB2 was mostly maintained after thermal degradation at decomposition temperature. For PN-PEB2 composite, the flexural strength (FS) and interlaminar shear strength (ILSS) were increased by 40.4 % and 44.8 % compared with the PN composite, respectively. After thermal degradation at 350 °C for 100 h, the FS retention rate of PN-PEB2 composite was 67.1 %.
KW - Mechanical properties
KW - Phthalonitrile resin
KW - Polymer-matrix composites (PMCs)
KW - Thermal degradation resistance
UR - https://www.scopus.com/pages/publications/85216559471
U2 - 10.1016/j.coco.2025.102272
DO - 10.1016/j.coco.2025.102272
M3 - 文章
AN - SCOPUS:85216559471
SN - 2452-2139
VL - 54
JO - Composites Communications
JF - Composites Communications
M1 - 102272
ER -