The effect of strain and low temperature sensitization on corrosion resistance of AISI 321 stainless steel in elevated borate buffer solution was investigated. The study found that the AISI 321 stainless steel with 20% strain showed the lowest degree of sensitization due to the fact that sample with 20% strain had high dislocation density which promoted chromium diffusion and a small amount of α'-martensites. The results from electrochemical impedance spectroscopy indicated that sensitized sample with 20% strain showed the best corrosion resistance after immersion test at 290 °C. A good agreement was found between the electrochemical impedance spectroscopy and the degree of sensitization. The oxide film was composed of three layers according to the results of the XPS and Raman spectra. In addition, the outer part compositions of the oxide film were mainly γ-Fe2O3and Fe-Cr spinel and iron hydroxide, while the inner and intermediate layers were mainly Fe-Cr spinel and the mixtures of the oxides of Fe, Cr, Ni. The ratio of hydroxide in oxide film increased due to large strain, especially for chromium hydroxide. Mott-Schottky analysis showed that more hydroxides induced more donor and acceptor concentrations in oxide film. More hydroxides reduced corrosion resistance of oxide film.

源语言英语
页(从-至)1235-1243
页数9
期刊Journal of Alloys and Compounds
696
DOI
出版状态已出版 - 2017

学术指纹

探究 'Characterization of the oxide films formed on low temperature sensitized AISI 321 stainless steel with different strain levels in elevated temperature borate buffer solution' 的科研主题。它们共同构成独一无二的学术指纹。

引用此