Analysis of failure of 316L heat exchanger in a producing glycine process using hydantoin method

  • Kui Xiao*
  • , Dan Wei
  • , Xin Zhang
  • , Xuequn Cheng
  • , Junsheng Wu
  • , Xiaogang Li
  • *此作品的通讯作者
  • University of Science and Technology Beijing
  • China University of Petroleum - Beijing
  • China Association for Science and Technology

科研成果: 书/报告/会议事项章节会议稿件同行评审

摘要

In this work, analysis was performed to investigate the reasons resulting in corrosion of 316L of heat exchanger tube in the producing glycine process. Results demonstrated that corrosion of 316L is attributed to intergranular corrosion of nonsensitized. Intergranular corrosion of nonsensitized occurs of 316L, the elements of Si, Ni, Mo are clustering, and the carbon oxide increases corrosion.

源语言英语
主期刊名New Materials and Advanced Materials
516-520
页数5
DOI
出版状态已出版 - 2011
已对外发布
活动2010 International Conference on Advances in Materials and Manufacturing Processes, ICAMMP 2010 - Shenzhen, 中国
期限: 6 11月 20108 11月 2010

出版系列

姓名Advanced Materials Research
152-153
ISSN(印刷版)1022-6680

会议

会议2010 International Conference on Advances in Materials and Manufacturing Processes, ICAMMP 2010
国家/地区中国
Shenzhen
时期6/11/108/11/10

学术指纹

探究 'Analysis of failure of 316L heat exchanger in a producing glycine process using hydantoin method' 的科研主题。它们共同构成独一无二的学术指纹。

引用此