Abstract
Adv. Mater. 2024, 36, 2404983 DOI: 10.1002/adma.202404983 When originally published, the SEM image of Figure S20D1 was incorrect: a duplicate of the SEM image of Figure S20C1 was shown. This error is caused by unintentional covering during the typesetting process. The corrected Figure S20 is shown below: S20 Figure (Figure presented.) SEM images of CNF with Li plating capacities of (A) 0, (B) 5, and (C) 10 mAh cm−2; Li stripping capacities of (D) 5 and (E) 10 mAh cm−2. Figure S20 shows the control sample of CNF, which has poor lithiophilicity. During the Li plating/stripping process, there is no obvious Li deposition behavior on the fiber surface at all times. Therefore, the arguments and conclusions of the original article are not affected. The authors apologize for any inconvenience caused.
| Original language | English |
|---|---|
| Article number | 2411621 |
| Journal | Advanced Materials |
| Volume | 36 |
| Issue number | 45 |
| DOIs |
|
| State | Published - 7 Nov 2024 |
Fingerprint
Dive into the research topics of 'Unveiling the In Situ Evolution of Li2O-Rich Solid Electrolyte Interface on CoOx Embedded Carbon Fibers as Li Anode Host'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver