Skip to main navigation Skip to search Skip to main content

The study on stress corrosion behavior of X65 steel welded joint in marine environment

  • University of Science and Technology Beijing

Research output: Chapter in Book/Report/Conference proceedingConference contributionpeer-review

Original languageEnglish
Title of host publicationEuropean Corrosion Congress, EUROCORR 2015
PublisherAustrian Society for Metallurgy and Materials (ASMET)
Pages1865
Number of pages1
ISBN (Electronic)9781510837379
StatePublished - 2015
Externally publishedYes
EventEuropean Corrosion Congress, EUROCORR 2015 - Graz, Austria
Duration: 6 Sep 201510 Sep 2015

Publication series

NameEuropean Corrosion Congress, EUROCORR 2015
Volume3

Conference

ConferenceEuropean Corrosion Congress, EUROCORR 2015
Country/TerritoryAustria
CityGraz
Period6/09/1510/09/15

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 14 - Life Below Water
    SDG 14 Life Below Water

Cite this