Abstract

Adopting electroplating process, a 10 μm palladium film was prepared on DD3 substrate. To examine the possibility of the palladium film used as the anti-diffusion layer between the bond coating and the substrate in the thermal barrier coating system, the 4 h and 14 h vacuum heat treatment at 1050 °C was carried out. The SEM/EDS study and the XRD analysis show that after vacuum heat treatment, the elements such as Al, Cr, Co, Ta and Ni diffuse outwards to the coating surface. And PdAl, α-Al2O3, and TiO2 are formed on the coating surface even under the vacuum condition. So Palladium film itself can not be used as the anti-diffusion layer between the substrate and the bond coating.

Original languageEnglish
Pages (from-to)1323-1326
Number of pages4
JournalXiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
Volume35
Issue number8
StatePublished - Aug 2006

Keywords

  • Diffusion
  • Pd
  • Superalloy
  • Thermal barrier coating