Abstract

The failure analysis for hot water pipes of 20 steel was performed by means of examinations of macro-morphology, metallograph and fractured surface, as well as chemical analysis and mechanical property measurement for the relevant materials. Results showed that the fracture occurred in the weld joints with obvious deterioration in weld area due to creep. The fracture initiated and propagated with typical brittle characteristics. The occurrence of corrosion products on cracking wall and in the cracking tip revealed that stress corrosion cracking (SCC) was the dominant factor of the pipe burst. Creep crack and fatigue characteristics were also found on the fracture, which accelerated the SCC and pipe burst.

Original languageEnglish
Pages (from-to)30-34
Number of pages5
JournalCorrosion Science and Protection Technology
Volume25
Issue number1
StatePublished - 2013
Externally publishedYes

Keywords

  • 20 steel
  • Burst
  • Hot-water pipe
  • SCC
  • Weld joint

Fingerprint

Dive into the research topics of 'Stress corrosion cracking failure of 20 steel used for hot water pipe'. Together they form a unique fingerprint.

Cite this