Skip to main navigation Skip to search Skip to main content

Stress corrosion cracking behavior and mechanism of high manganese steel in inshore SO2-polluted marine environment

  • Chao Li
  • , Jiahe Shi
  • , Yunhua Zhou
  • , Xiaokun Cai
  • , Tianqi Chen
  • , Yashun Feng
  • , Yunhua Huang*
  • , Xuequn Cheng
  • , Chao Liu*
  • , Xiaogang Li
  • *Corresponding author for this work
  • University of Science and Technology Beijing
  • Ltd.

Research output: Contribution to journalArticlepeer-review

Abstract

High manganese steel (HMS), widely utilized in railway transportation, often encounters the compounded challenge of high stress impact and corrosion, ultimately leading to environmentally assisted cracking. To comprehend this phenomenon, we delved into the stress corrosion cracking (SCC) behavior and mechanism of HMS in a SO2-polluted marine environment, employing both slow strain rate test (SSRT) and constant load U-bend test (CLUT). By comparing the SCC behavior in three distinct test solutions: 0.01 M NaHSO3, 0.01 M NaHSO3 with 1 wt% NaCl, and 0.01 M NaHSO3 with 3.5 wt% NaCl, we discerned the varied influence of Cl and SO2 on SCC. Analyzing the stress–strain curves from SSRT and the cross-sectional crack morphologies from CLUT provided insights into the SCC susceptibility of HMS in these solutions. Notably, the SCC susceptibility in 0.01 M NaHSO3 exceeded 40%, while in the solution containing 3.5 wt% NaCl, it significantly surpassed 65%. Further examination, including an analysis of the rust layer’s elemental distribution and phase composition, electrochemical testing of the rust layer, and an assessment of corrosion morphologies on the base metal, revealed the relative contributions of various corrosive media to SCC. This comprehensive study not only sheds light on potential SCC mechanisms but also offers valuable insights for evaluating the service life of HMS and identifying areas for performance optimization of this critical high manganese steel alloy.

Original languageEnglish
Pages (from-to)13146-13163
Number of pages18
JournalJournal of Materials Science
Volume59
Issue number28
DOIs
StatePublished - Jul 2024
Externally publishedYes

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 14 - Life Below Water
    SDG 14 Life Below Water

Fingerprint

Dive into the research topics of 'Stress corrosion cracking behavior and mechanism of high manganese steel in inshore SO2-polluted marine environment'. Together they form a unique fingerprint.

Cite this