SCC investigation of low alloy ultra-high strength steel 30CrMnSiNi2A in 3.5wt% NaCl solution by slow strain rate technique

  • Beihang University

Research output: Contribution to journalArticlepeer-review

Abstract

To evaluate stress corrosion cracking (SCC) mechanism of low alloy ultra-high strength steel 30CrMnSiNi2A in environment containing NaCl, SCC behavior of the steel in 3.5wt% NaCl solution is investigated by slow strain rate technique (SSRT) with various strain rates and applied potentials, surface analysis technique, and electrochemical measurements. SCC susceptibility of the steel increases rapidly with strain rate decreasing from 1 × 10-5 s-1 to 5 × 10-7 s-1, and becomes stable when strain rate is lower than 5 × 10-7 s-1. SCC propagation of the steel in the solution at open circuit potential (OCP) needs sufficient hydrogen which is supplied at a certain strain rate. Fracture surface at OCP has similar characteristics with that at cathodic polarization -1000 mVSCE, which presents characteristic fractography of hydrogen induced cracking (HIC). All of these indicate that SCC behavior of the steel in the solution at OCP is mainly controlled by HIC rather than anodic dissolution (AD).

Original languageEnglish
Pages (from-to)1327-1333
Number of pages7
JournalChinese Journal of Aeronautics
Volume27
Issue number5
DOIs
StatePublished - 2014

Keywords

  • Hydrogen
  • NaCl solution
  • Slow strain rate technique
  • Stress corrosion cracking
  • Ultra-high strength steel

Fingerprint

Dive into the research topics of 'SCC investigation of low alloy ultra-high strength steel 30CrMnSiNi2A in 3.5wt% NaCl solution by slow strain rate technique'. Together they form a unique fingerprint.

Cite this