Skip to main navigation Skip to search Skip to main content

Pore-induced fatigue failure: Critical pore criterion for Ti-6Al-4V alloy manufactured by laser-directed energy deposition

  • Linwei Dang
  • , Xiaofan He*
  • , Dingcheng Tang
  • , Hao Xin
  • , Xiangming Wang
  • , Bin Wu
  • , Liang Han
  • , Jinyu Wang
  • *Corresponding author for this work
  • Beihang University
  • China Aviation Industry Corporation

Research output: Contribution to journalArticlepeer-review

Abstract

Pores are the major factor inducing fatigue failure in laser-directed energy deposition (L-DED) Ti-6Al-4V alloy, posing obstacle to the application of the alloy in primary load-carrying components. Hence, it is essential to formulate criteria to identify critical pores that induce failure, an important step in evaluating the fatigue performance and predicting the fatigue life of L-DED Ti-6Al-4V alloy. In this paper, computed tomography was performed on tangentially blending fillets specimens to examine the distribution characteristics of pore geometric parameters, and location in the gauge section of the specimens. Then, fatigue experiments and fracture analysis were conducted. The results show that the location relative to the surface, size, and shape of the pores are the primary factors affecting fatigue failure. A stress state sensitive parameter was formulated by using location factors, projected area along the load direction, circularity of pores, and peak stress to establish a criterion for recognizing critical pores, the number of which can be reduced to two. The critical pore criterion based on stress state sensitive parameter was compared with those obtained via the other methods, proving its good applicability and effectiveness on identifying critical pores.

Original languageEnglish
Article number104204
JournalTheoretical and Applied Fracture Mechanics
Volume129
DOIs
StatePublished - Feb 2024

Keywords

  • Critical pore criterion
  • Fatigue failure
  • Laser-directed energy deposition
  • Stress state sensitive parameter

Fingerprint

Dive into the research topics of 'Pore-induced fatigue failure: Critical pore criterion for Ti-6Al-4V alloy manufactured by laser-directed energy deposition'. Together they form a unique fingerprint.

Cite this