Mitigated blistering and deuterium retention in tungsten exposed to high-flux deuterium-neon mixed plasmas

  • ITER
  • Trilateral Euregio Cluster
  • Max Planck Institute for Plasma Physics
  • Beijing University of Technology

Research output: Contribution to journalArticlepeer-review

Abstract

Surface morphology and deuterium retention in tungsten exposed at surface temperature of ∼550 K to mixed deuterium-neon plasmas of different neon concentrations are investigated. It is found that the addition of neon up to 20% mitigates blistering on the surface. Cross-section view of the surface shows the formation of pores near the surface in the depth less than 100 nm. Deuterium depth profile is featured by an enhanced deuterium concentration within a depth of 16 nm but a mitigated penetration in depth larger than 1 μm. Deuterium retention is reduced by up to a factor of four. It is suggested the open pores formed in the surface serves as an escaping channel, mitigates deuterium penetration towards bulk and retention in the bulk.

Original languageEnglish
Article number046028
JournalNuclear Fusion
Volume57
Issue number4
DOIs
StatePublished - 10 Mar 2017

Keywords

  • deuterium retention
  • neon
  • plasma-material interaction
  • tungsten

Fingerprint

Dive into the research topics of 'Mitigated blistering and deuterium retention in tungsten exposed to high-flux deuterium-neon mixed plasmas'. Together they form a unique fingerprint.

Cite this