Mechanism and evaluation method of stress corrosion susceptibility of 904L stainless steel with optimized structure in seawater

  • Di Xu
  • , Xianwei Zhang
  • , Xin He
  • , Chao Liu*
  • , Zhiyong Liu
  • , Xin Zhang
  • , Mengjing Zhao
  • , Xiaogang Li
  • *Corresponding author for this work
  • University of Science and Technology Beijing
  • State Power Investment Corporation Limited
  • China International Engineering Consulting Corporation

Research output: Contribution to journalArticlepeer-review

Abstract

The stress corrosion cracking (SCC) and the electrochemical behavior of 904 L stainless steel in a simulated seawater environment were investigated using slow strain rate testing (SSRT), electrochemical polarization, electrochemical impedance spectroscopy (EIS) and Mott-Schottky (M-S) curves. The sensitive potential range of 904 L stainless steel was determined by the fast and slow scan potential polarization curve, is − 950 mVSCE ∼ 270 mVSCE. Moreover, with the negative shift of applied potential, the toughness fracture characteristic of the three kinds of steel is reduced, and the sensitization state steel is the most obvious reduction. Finally, a practical formula for evaluating the SCC susceptibility of 904 L stainless steel was developed by integrating data from SSRT and fast and slow scan polarization curves.

Original languageEnglish
Article number111865
JournalCorrosion Science
Volume229
DOIs
StatePublished - 1 Apr 2024
Externally publishedYes

Keywords

  • 904L stainless steel
  • Electrochemical character, SCC susceptibility evaluation method
  • Stress corrosion cracking