Iron-rich 2:17-type SmCo magnets are expected to achieve high performance and relatively low cost. However, inhomogeneous cellular structures usually exist in iron-rich magnets, resulting in a drastic reduction in coercivity and energy product. Herein, a strategy is proposed to regulate the dislocation by decreasing the Sm content and extending the solid-solution duration in precursor of iron-rich SmCo magnet. High-density dislocations in precursor contributed to 1:5H nucleation, leading to uniform cellular structures in final magnets. As a result, a remarkable intrinsic coercivity of 1.50 T and one of the highest remanences (1.24 T) are simultaneously achieved in the iron-rich Sm25Co42Fe26Cu5Zr2 (wt%) magnet. This study provides valuable insights into the design and development of iron-rich 2:17-type SmCo magnets.

Original languageEnglish
Article number2400305
JournalAdvanced Functional Materials
Volume34
Issue number33
DOIs
StatePublished - 14 Aug 2024

Keywords

  • dislocations
  • intrinsic coercivities
  • iron-rich SmCo magnets
  • remanences
  • solid-solution precursors

Fingerprint

Dive into the research topics of 'Large Coercivity and High Remanence in Iron-Rich 2:17-Type SmCo Magnets:Effect of Dislocation on Solid-Solution Precursors'. Together they form a unique fingerprint.

Cite this