Abstract
Welding of Cf/SiC to Ni-based superalloy has been realized using Cu/W/Cu/W/Cu multiple interlayers. The bending strength of the joints has been improved by using the active metallic filler contacted with Cf/SiC. The strength of the joints is remarkably affected by the welding temperature. The maximum value 102.1 MPa has been obtained at 970°C (dwell time: 10 min., welding pressure: 34.3 MPa). Microstructural studies were also conducted.
| Original language | English |
|---|---|
| Pages (from-to) | 1777-1781 |
| Number of pages | 5 |
| Journal | International Journal of Modern Physics B |
| Volume | 17 |
| Issue number | 8-9 II |
| DOIs | |
| State | Published - 10 Apr 2003 |