We report enhanced thermoelectric performance in SnTe, where significantly improved electrical transport properties and reduced thermal conductivity were achieved simultaneously. The former was obtained from a larger hole Seebeck coefficient through Fermi level tuning by optimizing the carrier concentration with Ga, In, Bi, and Sb dopants, resulting in a power factor of 21 μW cm-1 K-2 and ZT of 0.9 at 823 K in Sn0.97Bi0.03Te. To reduce the lattice thermal conductivity without deteriorating the hole carrier mobility in Sn0.97Bi0.03Te, SrTe was chosen as the second phase to create strained endotaxial nanostructures as phonon scattering centers. As a result, the lattice thermal conductivity decreases strongly from ∼2.0 Wm-1 K-1 for Sn0.97Bi0.03Te to ∼1.2 Wm-1 K-1 as the SrTe content is increased from 0 to 5.0% at room temperature and from ∼1.1 to ∼0.70 Wm-1 K-1 at 823 K. For the Sn0.97Bi0.03Te-3% SrTe sample, this leads to a ZT of 1.2 at 823 K and a high average ZT (for SnTe) of 0.7 in the temperature range of 300-823 K, suggesting that SnTe is a robust candidate for medium-temperature thermoelectric applications.

Original languageEnglish
Pages (from-to)2366-2373
Number of pages8
JournalJournal of the American Chemical Society
Volume138
Issue number7
DOIs
StatePublished - 2 Mar 2016

Fingerprint

Dive into the research topics of 'Enhanced Thermoelectric Properties in the Counter-Doped SnTe System with Strained Endotaxial SrTe'. Together they form a unique fingerprint.

Cite this