Skip to main navigation Skip to search Skip to main content

Effect of hot rolling on corrosion resistance of Cu-7Ni-3Al-1Fe-1Mn-0.02Sm alloy

  • Lanqing Niu
  • , Shuguo Jia*
  • , Shizhong An
  • , Kexing Song
  • , Haitao Liu
  • , Chu Cheng
  • , Bo Wang
  • , Nuoya Wang
  • , Deqing Niu
  • *Corresponding author for this work
  • Henan University of Science and Technology
  • Jointly Built by The Ministry
  • Henan Key Laboratory of Nonferrous Materials Science and Processing Technology
  • Henan Academy of Sciences
  • Nanyang Normal University

Research output: Contribution to journalArticlepeer-review

Abstract

Improving the corrosion resistance of copper-nickel alloy is crucial to extend its service life in marine engineering. In this study, hot rolling was used to improve the corrosion resistance of the alloy, and the reasons for the improvement of corrosion resistance were explored. The corrosion rate of the alloy was reduced by 89% from 0.0150 mm/a to 0.0017 mm/a when the deformation amount is 80%. The improved corrosion resistance can be attributed to two reasons: (1) hot rolling promotes the formation of dense Cu2O film in the corrosion product, reduces the content of loose Cu2(OH)3Cl, making the corrosion product film more compact, (2) Fe, Ni and Sm elements involved in the formation of the corrosion product film, generated Sm-S phase, γ-FeOOH and Ni(OH)2, making the corrosion potential shift positively. This work proposes an alternative approach to enhance the corrosion resistance of copper alloys.

Original languageEnglish
Pages (from-to)111-122
Number of pages12
JournalCorrosion Engineering Science and Technology
Volume61
Issue number2
DOIs
StatePublished - Mar 2026
Externally publishedYes

Keywords

  • Hot rolling
  • copper nickel alloy
  • corrosion resistance
  • corrosive film
  • deformation amount

Fingerprint

Dive into the research topics of 'Effect of hot rolling on corrosion resistance of Cu-7Ni-3Al-1Fe-1Mn-0.02Sm alloy'. Together they form a unique fingerprint.

Cite this