Abstract
Anodic aluminum oxide (AAO) membranes with large ordered pore domains were successfully prepared by adopting the anneal pre-treatment of polycrystalline aluminum sheets. A statistical method with Gaussian distribution was introduced to quantitatively study the size of the domain with ordered pores. The largest average area of ordered pore domains was 2.6 μm2±0.11 μm2. The corresponding AAO membrane was synthesized by aluminum sheets annealed at 893 K for 24 h.
| Original language | English |
|---|---|
| Pages (from-to) | 1838-1842 |
| Number of pages | 5 |
| Journal | Science in China, Series E: Technological Sciences |
| Volume | 51 |
| Issue number | 11 |
| DOIs | |
| State | Published - Nov 2008 |
| Externally published | Yes |
Keywords
- Annealing duration
- Annealing temperature
- Anodic aluminum oxide (AAO)
- Gaussian distribution
Fingerprint
Dive into the research topics of 'Effect of anneal pre-treatment of polycrystalline aluminum sheets on synthesis of highly-ordered anodic aluminum oxide membranes'. Together they form a unique fingerprint.Cite this