Deformation morphology underneath the vickers indent in bulk metallic glasses

  • CAS - Institute of Mechanics
  • Tianjin Normal University

Research output: Contribution to journalArticlepeer-review

Abstract

Plastic deformation behaviour of Zr52.5Al10Ni 10Cu15Be12.5 and Mg65Cu 25Gd10 bulk metallic glasses (BMGs) is studied by using the depth-sensing nanoindentation and microindentation. The subsurface plastic deformation zone of the BMGs is investigated using the bonded interface technique. Both the BMGs exhibit the serrated flow depending on the loading rate in the loading process of indentation. Slow indentation rates promote more conspicuous serrations, and rapid indentations suppress the serrated flow. Mg-based BMG shows a much higher critical loading rate for the disappearance of the serration than that in Zr-based BMG. The significant difference in the shear band pattern in the subsurface plastic deformation zone is responsible for the different deformation behaviour between the two BMGs. Increase of the loading rate can lead to the increase of the density of shear bands. However, there is no distinct change in the character of shear bands at the loading rate of as high as 1000 nm/s.

Original languageEnglish
Pages (from-to)1994-1997
Number of pages4
JournalChinese Physics Letters
Volume22
Issue number8
DOIs
StatePublished - 1 Aug 2005
Externally publishedYes

Fingerprint

Dive into the research topics of 'Deformation morphology underneath the vickers indent in bulk metallic glasses'. Together they form a unique fingerprint.

Cite this