La2CuO4 and La1.86Sr0.14CuO4 single crystals were obtained by traveling solvent floating zone method. There were five kinds of defects in these single crystals: cracks, inclusions, gas bubbles, unhomogeneous distribution of Sr2+, and substructures. CH3COOH aqueous solution was used to etch these single crystals, and the etch-pit density was calculated. The formation mechanism of these defects was discussed. It is suggested that the good preparation of raw materials and the stringent growth conditions play an important role in growing high quality single crystals.

Original languageEnglish
Pages (from-to)71-75
Number of pages5
JournalRare Metals
Volume24
Issue number1
StatePublished - Mar 2005

Keywords

  • Defect
  • Etch-pit density
  • Traveling solvent floating zone method

Fingerprint

Dive into the research topics of 'Defects in La2CuO4 and La1.86Sr0.14CuO4 single crystals'. Together they form a unique fingerprint.

Cite this