Abstract

The electrochemical corrosion and stress corrosion cracking (SCC) behaviors of X70 pipeline steel in CO 2-containing solution were studied by electrochemical measurements, slow strain rate tensile tests, and surface characterization. The results found that the electrochemical corrosion of X70 steel in aerated, alkaline solution is an activation-controlled process, and a stable passivity cannot develop on steel. Corrosion rate of the steel increases with the CO 2 partial pressure. The enhanced anodic dissolution due to the additional cathodic reaction in the presence of CO 2, rather than the film-formation reaction, dominates the corrosion process. The mass-transfer step through FeCO 3 deposit is the rate-controlling step in corrosion of the steel. The susceptibility of steel to SCC and the fracture brittleness increase with the CO 2 partial pressure. The enhanced fracture brittleness is attributed to the evolution and penetration of hydrogen atoms into the steel, contributing to crack propagation. The formed deposit layer is not effective in reducing hydrogen permeation due to the loose, porous structure.

Original languageEnglish
Pages (from-to)319-323
Number of pages5
JournalJournal of Materials Engineering and Performance
Volume18
Issue number3
DOIs
StatePublished - Apr 2009
Externally publishedYes

Keywords

  • CO
  • Corrosion
  • Pipeline steel
  • Stress corrosion cracking

Fingerprint

Dive into the research topics of 'Corrosion and stress corrosion cracking behavior of X70 pipeline steel in a CO 2-containing solution'. Together they form a unique fingerprint.

Cite this