Abstract
Based on the results of thermochemical analysis, NH4I+NH4Cl proved to be a more favorable activator for codepositing Co-Al-Y compared to NH4I or NH4Cl. Coating deposition experiments were also demonstrated that codeposition of Co-Al-Y with high concentration of Co and minute quantities of Y could be achieved at 1323K in the NH4I+NH4Cl activated packs. The coating exhibited the best cyclic oxidation resistance at 1323K when NH4I+NH4Cl were used as activator.
| Original language | English |
|---|---|
| Pages (from-to) | 454-460 |
| Number of pages | 7 |
| Journal | Corrosion Science |
| Volume | 75 |
| DOIs | |
| State | Published - Oct 2013 |