Abstract
Dissimilar metallic materials find broad applications owing to the possibility of integrating multiple functions. However, the joining interface is a vulnerable site for failure in service. The design of high-strength bonding of dissimilar materials has been urgently needed. This study showed that a combination of additive friction stir deposition coupled with post-processing annealing enables the formation of a continuous Mg/O-enriched amorphous layer dotted with nano-rivet structures at the aluminum (Al)/steel interface. As a result, a high bonding strength (138.1 MPa) of Al/steel was achieved. We clarify the formation of discontinuous nano-rivet intermetallic compounds thanks to the AFSD-induced severe plastic deformation and local chemical reaction upon annealing, and we demonstrate the highest bonding strength is achieved at the size of nano-rivet compounds of ~200 nm and the aspect ratio ~ 0.5. Our findings provide a simple but versatile strategy to reverse the adverse effects of intermetallic compounds on the interface strength of dissimilar materials.
| Original language | English |
|---|---|
| Pages (from-to) | 491-502 |
| Number of pages | 12 |
| Journal | Journal of Manufacturing Processes |
| Volume | 133 |
| DOIs | |
| State | Published - 17 Jan 2025 |
Keywords
- Additive friction stir deposition
- Al/steel
- High bonding strength
- Interface
- Nano-rivet structure
Fingerprint
Dive into the research topics of 'Aluminum/steel dissimilar material with high interfacial strength manufactured by additive friction stir deposition'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver